105WCr6 Tool Die Steels to DIN 17350 (1980)

105WCr6 - Specification & Application

  • DIN 17350 (1980) - Tool Steels; Technical Conditions of Delivery

Tool Steels; Technical Conditions of Delivery

Chemical composition(wt.%) of 105WCr6 grade: to DIN 17350 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.00 1.10
Si 0.10 0.40
Mn 0.80 1.10
P - 0.030
S - 0.030
Cr 0.90 1.10
Mo - -
V - -
W 1.00 1.30

105WCr6 - Detail

Tool Steels; Technical Conditions of Delivery

Mechanical properties of grade 105WCr6 DIN 17350 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
969 (≥) 669 (≥) 24 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade 105WCr6 DIN 17350 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
851 (≥) 318 (≥) 41 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
312 995 322

Equivalent Grade

Equivalent Products