10CrMo9-10 Stainless Steels to EN 10028-2: 2009

10CrMo9-10 - Specification & Application

  • EN 10028-2: 2009 - Flat products made of steels for pressure purposes. Non-alloy and alloy steels with specified elevated temperature properties
  • EN 10216-2: 2014 - Seamless steel tubes for pressure purposes. Technical delivery conditions. Non-alloy and alloy steel tubes with specified elevated temperature properties
  • EN 10253-2: 2007 - Butt-welding pipe fittings. Non alloy and ferritic alloy steels with specific inspection requirements
  • EN 10273: 2007 - Hot rolled weldable steel bars for pressure purposes with specified elevated temperature properties

Alloy special steel

Chemical composition(wt.%) of 10CrMo9-10 grade: to EN 10028-2: 2009

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.14
Si - 0.5
Mn 0.4 0.8
P - 0.020
S - 0.010
Cr 2.00 2.50
Mo 0.90 1.10
N - 0.012
Cu - 0.3

10CrMo9-10 - Detail

10CrMo9-10

Mechanical properties of grade 10CrMo9-10 EN 10028-2: 2009

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
945 (≥) 426 (≥) 32 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade 10CrMo9-10 EN 10028-2: 2009

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
334 (≥) 254 (≥) 23 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
516 466 831

Equivalent Products

We can customize the production of 10CrMo9-10 grade, contact us for the best solution.