15CDV6 Air 9160/C Aviation and Aero Steel to AIR 9160 C

15CDV6 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of 15CDV6 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.12 0.18
Si - 0.20
Mn 0.80 1.10
P - 0.020
S - 0.015
Cr 1.25 1.50
Mo 0.80 1.00
V 0.20 0.30

15CDV6 Air 9160/C - Detail

XC65 XC-65 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade 15CDV6 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
993 (≥) 974 (≥) 33 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade 15CDV6 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
915 (≥) 794 (≥) 23 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
397 932 542
We can customize the production of 15CDV6 Air 9160/C grade, contact us for the best solution.
sales@specificsteel.com