1Cr18Ni9Ti Stainless Steels to GB 13296 (2007)

1Cr18Ni9Ti - Specification & Application

  • GB 13296 (2007) - Seamless stainless steel tubes for boiler and heat exchanger
  • GB 2270 (1980) - Seamless tubes
  • GB 4238 (1992) - Heat-resisting steel sheets and plates
  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 1221 (1992) - Heat-resisting steel bars
  • GB/T 12770 (2002) - Welded stainless steel tubes for machine structures
  • GB/T 12771 (2000) - Welded stainless steel pipes for liquid delivery
  • GB/T 14975 (2002) - Stainless steel seamless tubes for structures
  • GB/T 14976 (2002) - Stainless steel seamless tubes for fluid transport
  • GB/T 3089 (1982) - Thinnest-wall seamless tubes of stainless and acid-resistance steel
  • GB/T 3090 (2000) - Stainless steel small diameter seamless steel tubes
  • GB/T 3280 (1992) - Cold rolled stainless steel sheets and plates
  • GB/T 4226 (2004) - Cold finished stainless steel bars
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips
  • GB/T 4240 (1993) - Stainless steel wires
  • GB/T 4356 (2002) - Stainless steel wire rods
  • JB 4728 (2000) - Stainless steel forgings for pressure vessels
  • JB/T 6398 (2006) - Heavy stainless acid resistant and heat resistant steel forgings

Seamless stainless steel tubes for boiler and heat exchanger

Chemical composition(wt.%) of 1Cr18Ni9Ti grade: to GB 13296 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 8.00 11.00
Cr 17.00 19.00
Ti - 5x(C%-0.02)-0.80

1Cr18Ni9Ti - Detail

1Cr18Ni9Ti

Mechanical properties of grade 1Cr18Ni9Ti GB 13296 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
141 (≥) 988 (≥) 12 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade 1Cr18Ni9Ti GB 13296 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
758 (≥) 735 (≥) 24 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
971 647 532

Equivalent Grade

Equivalent Products

We can customize the production of 1Cr18Ni9Ti grade, contact us for the best solution.
sales@specificsteel.com