1Cr20Ni14Si2 Stainless Steels to GB 4238 (1992)

1Cr20Ni14Si2 - Specification & Application

  • GB 4238 (1992) - Heat-resisting steel sheets and plates
  • GB/T 1221 (1992) - Heat-resisting steel bars

Heat-resisting steel sheets and plates

Chemical composition(wt.%) of 1Cr20Ni14Si2 grade: to GB 4238 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si 1.50 2.50
Mn - 1.50
P - 0.035
S - 0.030
Ni 12.00 15.00
Cr 19.00 22.00

1Cr20Ni14Si2 - Detail

1Cr20Ni14Si2

Mechanical properties of grade 1Cr20Ni14Si2 GB 4238 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
219 (≥) 958 (≥) 12 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 1Cr20Ni14Si2 GB 4238 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
894 (≥) 334 (≥) 33 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
597 144 576

Equivalent Grade

Equivalent Products

We can customize the production of 1Cr20Ni14Si2 grade, contact us for the best solution.