2303 Stainless Steels to SS 142303

2303 - Specification & Application

  • SS 142303 - Stainless steel - SS steel 2303

Stainless steel - SS steel 2303

Chemical composition(wt.%) of 2303 grade: to SS 142303

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16 0.25
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 12.00 14.00
Ni - 1.00
Mo - -

2303 - Detail

Stainless steel - SS steel 2303

Mechanical properties of grade 2303 SS 142303

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
366 (≥) 282 (≥) 44 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade 2303 SS 142303

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
377 (≥) 598 (≥) 43 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
919 762 292

Equivalent Grade

Equivalent Products

We can customize the production of 2303 grade, contact us for the best solution.