2368 Stainless Steels to SS 142368

2368 - Specification & Application

  • SS 142368 - Stainless steel - SS steel 2368

Stainless steel - SS steel 2368

Chemical composition(wt.%) of 2368 grade: to SS 142368

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Si 1.40 2.00
Mn - 0.80
P - 0.040
S - 0.030
Cr 20.00 22.00
Ni 10.00 12.00
Mo - -
N 0.14 0.20
Ce 0.03 0.08

2368 - Detail

Stainless steel - SS steel 2368

Mechanical properties of grade 2368 SS 142368

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
244 (≥) 438 (≥) 34 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 2368 SS 142368

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
826 (≥) 771 (≥) 24 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
565 135 456