2372 Stainless Steels to SS 142372

2372 - Specification & Application

  • SS 142372 - Stainless steel - SS-steel 2372

Stainless steel - SS-steel 2372

Chemical composition(wt.%) of 2372 grade: to SS 142372

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.06
Si 1.00 2.00
Mn - 0.80
P - 0.040
S - 0.030
Cr 18.00 19.00
Ni 9.00 10.00
Mo - -
N 0.12 0.18
Ce 0.03 0.08

2372 - Detail

Stainless steel - SS-steel 2372

Mechanical properties of grade 2372 SS 142372

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
413 (≥) 681 (≥) 13 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade 2372 SS 142372

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
817 (≥) 564 (≥) 43 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
581 218 656

Equivalent Grade

Equivalent Products

We can customize the production of 2372 grade, contact us for the best solution.