2Cr25Ni20 Stainless Steels to GB 13296 (2007)

2Cr25Ni20 - Specification & Application

  • GB 13296 (2007) - Seamless stainless steel tubes for boiler and heat exchanger
  • GB 4238 (1992) - Heat-resisting steel sheets and plates
  • GB/T 1221 (1992) - Heat-resisting steel bars
  • JB/T 6398 (2006) - Heavy stainless acid resistant and heat resistant steel forgings

Seamless stainless steel tubes for boiler and heat exchanger

Chemical composition(wt.%) of 2Cr25Ni20 grade: to GB 13296 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - 1.50
Mn - 2.00
P - 0.35
S - 0.03
Ni 19.00 22.00
Cr 24.00 26.00

2Cr25Ni20 - Detail

2Cr25Ni20

Mechanical properties of grade 2Cr25Ni20 GB 13296 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
612 (≥) 683 (≥) 31 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade 2Cr25Ni20 GB 13296 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
957 (≥) 157 (≥) 44 14 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
853 182 474

Equivalent Grade

Equivalent Products

We can customize the production of 2Cr25Ni20 grade, contact us for the best solution.
sales@specificsteel.com