303 Stainless Steels to A 314 (2008)

303 - Specification & Application

  • A 314 (2008) - Stainless Steel Billets and Bars for Forging
  • A 473 (2009) - Stainless Steel Forgings
  • A 581/A 581M (2009) - Free-Machining Stainless Steel Wire and Wire Rods
  • A 582/A 582M (2012) - Free-Machining Stainless Steel Bars
  • A 895 (2009) - Free-Machining Stainless Steel Plate, Sheet, and Strip
  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Stainless Steel Billets and Bars for Forging

Chemical composition(wt.%) of 303 grade: to A 314 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.2
S 0.15 -
Cr 17.0 19.0
Ni 8.00 10.0
Mo - 0.60

303 - Detail

Stainless Steel Billets and Bars for Forging

Mechanical properties of grade 303 A 314 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
347 (≥) 458 (≥) 31 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 303 A 314 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
545 (≥) 415 (≥) 42 24 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
242 184 264

Equivalent Products

We can customize the production of 303 grade, contact us for the best solution.
sales@specificsteel.com