316F20 Stainless Steels to NF A 49-214

316F20 - Specification & Application

  • NF A 49-214 - Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery

Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery

Chemical composition(wt.%) of 316F20 grade: to NF A 49-214

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 16.00 18.00
Ni 11.00 13.00
Mo 2.00 2.50
B 0.0015 0.0060

316F20 - Detail

Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery

Mechanical properties of grade 316F20 NF A 49-214

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
444 (≥) 662 (≥) 11 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade 316F20 NF A 49-214

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
276 (≥) 922 (≥) 31 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
524 983 728

Equivalent Products

We can customize the production of 316F20 grade, contact us for the best solution.