317J1 Stainless Steels to G3067

317J1 - Specification & Application

  • G3067 - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of 317J1 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.00
Mn - 2.50
P - 0.045
S - 0.030
Ni 15.00 17.00
Cr 16.00 19.00
Mo 4.00 6.00

317J1 - Detail

Stainless steel bars

Mechanical properties of grade 317J1 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
873 (≥) 219 (≥) 24 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade 317J1 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
251 (≥) 448 (≥) 32 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
245 547 373

Equivalent Products

We can customize the production of 317J1 grade, contact us for the best solution.