32CrMoV12-10 / 32CDV12 Tool Die Steels

32CrMoV12-10 / 32CDV12 - Specification & Application

Chemical composition(wt.%) of 32CrMoV12-10 / 32CDV12 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C(CarBon) - 0.35
Cr - 3.0
Mo - 1.0
V - 0.25

32CrMoV12-10 / 32CDV12 - Detail

32CrMoV12-10

Mechanical properties of grade 32CrMoV12-10 / 32CDV12

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
763 (≥) 479 (≥) 42 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade 32CrMoV12-10 / 32CDV12

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
322 (≥) 773 (≥) 21 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
748 675 327

Equivalent Products

We can customize the production of 32CrMoV12-10 / 32CDV12 grade, contact us for the best solution.