40CrMnMo7 Tool Die Steels to SE 201 (1992)

40CrMnMo7 - Specification & Application

  • SE 201 (1992) - Materials for tubes and tools for the extrusion processing of copper and copper alloys
  • SE 202 (1995) - Heat resistant materials for the extrusion processing of aluminum and aluminum alloys

Heat resistant materials for the extrusion processing of aluminum and aluminum alloys

Chemical composition(wt.%) of 40CrMnMo7 grade: to SE 201 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 0.20 0.40
Mn 1.30 1.60
P - 0.035
S - 0.035
Cr 1.80 2.10
Mo 0.15 0.25
V - -

40CrMnMo7 - Detail

Heat resistant materials for the extrusion processing of aluminum and aluminum alloys

Mechanical properties of grade 40CrMnMo7 SE 201 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
549 (≥) 833 (≥) 23 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade 40CrMnMo7 SE 201 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
824 (≥) 663 (≥) 11 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
211 769 728

Equivalent Products

We can customize the production of 40CrMnMo7 grade, contact us for the best solution.