632J1CPS Stainless Steels

632J1CPS - Specification & Application

CNS standard spring cold rolled stainless steel strip

Chemical composition(wt.%) of 632J1CPS grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si 1.00 2.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 13.50 15.50
Ni 6.50 7.55
Cu 0.40 1.00
Ti 0.20 0.65

632J1CPS - Detail

CNS standard spring cold rolled stainless steel strip

Mechanical properties of grade 632J1CPS

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
522 (≥) 211 (≥) 21 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade 632J1CPS

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
426 (≥) 843 (≥) 41 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
387 442 931

Equivalent Grade

Equivalent Products

We can customize the production of 632J1CPS grade, contact us for the best solution.