6F5 Tool Die Steels

6F5 - Specification & Application

Mold Steel

Chemical composition(wt.%) of 6F5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.55
Si - 1.00
Mn - 1.00
Cr - 0.50
Mo - 0.50
V - 0.10
W - -
Ni - 2.70

6F5 - Detail

Mold Steel

Mechanical properties of grade 6F5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
689 (≥) 594 (≥) 13 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade 6F5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
233 (≥) 589 (≥) 31 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
796 374 818

Equivalent Grade

Equivalent Products

We can customize the production of 6F5 grade, contact us for the best solution.
sales@specificsteel.com