75Cr1 Tool Die Steels to DIN 17350

75Cr1 - Specification & Application

  • DIN 17350 - Tool Steels; Technical Conditions of Delivery

Tool Steels; Technical Conditions of Delivery

Chemical composition(wt.%) of 75Cr1 grade: to DIN 17350

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.70 0.80
Si 0.25 0.50
Mn 0.60 0.80
P - 0.030
S - 0.030
Cr 0.30 0.40
Mo - -
V - -

75Cr1 - Detail

Tool Steels; Technical Conditions of Delivery

Mechanical properties of grade 75Cr1 DIN 17350

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
473 (≥) 815 (≥) 34 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade 75Cr1 DIN 17350

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
153 (≥) 857 (≥) 12 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
192 573 587

Equivalent Grade

Equivalent Products

We can customize the production of 75Cr1 grade, contact us for the best solution.