A 167 Type 310Cb Stainless Steels to A 167 (1999)

A 167 Type 310Cb - Specification & Application

  • A 167 (1999) - Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of A 167 Type 310Cb grade: to A 167 (1999)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Nb+Ta - 1.10

A 167 Type 310Cb - Detail

Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Mechanical properties of grade A 167 Type 310Cb A 167 (1999)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
919 (≥) 973 (≥) 32 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade A 167 Type 310Cb A 167 (1999)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
411 (≥) 772 (≥) 14 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
228 693 651