A 182 F XM-11 Stainless Steels to A 182/A 182M (2012)

A 182 F XM-11 - Specification & Application

  • A 182/A 182M (2012) - Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Chemical composition(wt.%) of A 182 F XM-11 grade: to A 182/A 182M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.00
Mn 8.00 10.0
P - 0.06
S - 0.03
Cr 19.0 21.5
Ni 5.50 7.50
N 0.15 0.40

A 182 F XM-11 - Detail

A 182 F XM-11

Mechanical properties of grade A 182 F XM-11 A 182/A 182M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
493 (≥) 844 (≥) 31 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade A 182 F XM-11 A 182/A 182M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
479 (≥) 582 (≥) 43 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
175 485 231

Equivalent Products