A 313 Type XM-28 Stainless Steels to A 313/A 313M (2010)

A 313 Type XM-28 - Specification & Application

  • A 313/A 313M (2010) - Stainless Steel Spring Wire

Stainless Steel Bars and Shapes

Chemical composition(wt.%) of A 313 Type XM-28 grade: to A 313/A 313M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 11.0 14.0
P - 0.045
S - 0.030
Si - 1.00
Ni 0.5 2.5
Cr 16.5 19.00
N 0.20 0.45

A 313 Type XM-28 - Detail

A 313 Type XM-28

Mechanical properties of grade A 313 Type XM-28 A 313/A 313M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
882 (≥) 717 (≥) 23 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade A 313 Type XM-28 A 313/A 313M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
229 (≥) 714 (≥) 23 42 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
564 934 438

Equivalent Products

We can customize the production of A 313 Type XM-28 grade, contact us for the best solution.
sales@specificsteel.com