A 368 S30200 Stainless Steels to A 368 (2009)

A 368 S30200 - Specification & Application

  • A 368 (2009) - Stainless Steel Wire Strand

Stainless Steel Wire Strand

Chemical composition(wt.%) of A 368 S30200 grade: to A 368 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 17.0 19.0
Ni 8.00 10.00

A 368 S30200 - Detail

Composed of a multiplicity of round wires and suitable for use as guy wires, overhead ground wires, and similar purposes.  
The material shall be supplied in the cold drawn condition. 

Mechanical properties of grade A 368 S30200 A 368 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
345 (≥) 276 (≥) 24 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade A 368 S30200 A 368 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
486 (≥) 874 (≥) 14 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
746 815 958

Equivalent Products

We can customize the production of A 368 S30200 grade, contact us for the best solution.
sales@specificsteel.com