A 492 S21603 Stainless Steels to A 492 (2009)

A 492 S21603 - Specification & Application

  • A 492 (2009) - Stainless Steel Rope Wire

Stainless Steel Rope Wire

Chemical composition(wt.%) of A 492 S21603 grade: to A 492 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn 7.50 9.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.50 22.00
Ni 7.50 9.00
Mo 2.00 3.00
N 0.25 0.50

A 492 S21603 - Detail

Stainless Steel Rope Wire

Mechanical properties of grade A 492 S21603 A 492 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
847 (≥) 644 (≥) 21 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade A 492 S21603 A 492 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
346 (≥) 122 (≥) 11 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
561 283 316

Equivalent Products

We can customize the production of A 492 S21603 grade, contact us for the best solution.
sales@specificsteel.com