A 580 Type XM-29 Stainless Steels to A 580/A 580M (2012)

A 580 Type XM-29 - Specification & Application

  • A 580/A 580M (2012) - Stainless Steel Wire

Stainless Steel Wire

Chemical composition(wt.%) of A 580 Type XM-29 grade: to A 580/A 580M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn 11.5 14.5
P - 0.06
S - 0.03
Cr 17.0 19.0
Ni 2.25 3.75
N 0.20 0.40

A 580 Type XM-29 - Detail

A 580 Type XM-29

Mechanical properties of grade A 580 Type XM-29 A 580/A 580M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
662 (≥) 181 (≥) 11 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade A 580 Type XM-29 A 580/A 580M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
272 (≥) 234 (≥) 32 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
797 936 365

Equivalent Products

We can customize the production of A 580 Type XM-29 grade, contact us for the best solution.