A 688 Grade TP 304N Stainless Steels to A 688/A 688M (2012)

A 688 Grade TP 304N - Specification & Application

  • A 688/A 688M (2012) - Welded Austenitic Stainless Steel Feedwater Heater Tubes

Welded Austenitic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of A 688 Grade TP 304N grade: to A 688/A 688M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 10.5
N 0.10 0.16

A 688 Grade TP 304N - Detail

Welded Austenitic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade A 688 Grade TP 304N A 688/A 688M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
847 (≥) 159 (≥) 11 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade A 688 Grade TP 304N A 688/A 688M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
174 (≥) 683 (≥) 42 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
727 329 142

Equivalent Products

We can customize the production of A 688 Grade TP 304N grade, contact us for the best solution.
sales@specificsteel.com