A 959 S21500 Stainless Steels to A 959 (2011)

A 959 S21500 - Specification & Application

  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Chemical composition(wt.%) of A 959 S21500 grade: to A 959 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 5.50 7.00
Si - 1.20
P - 0.04
S - 0.03
Cr 14.00 16.00
Ni 9.00 11.00
Mo - -
B 0.003 0.009
Nb 0.75 1.25
V 0.15 0.40

A 959 S21500 - Detail

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Mechanical properties of grade A 959 S21500 A 959 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
714 (≥) 141 (≥) 32 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade A 959 S21500 A 959 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
562 (≥) 845 (≥) 24 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
153 615 688

Equivalent Products

We can customize the production of A 959 S21500 grade, contact us for the best solution.
sales@specificsteel.com