A3 Special Alloy

Chemical composition%of the ladle analysis of gradeA3

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Mo(%)V(%)
1.20~1.300.10~0.500.40~0.60≤0.030≤0.0304.75~5.500.90~1.400.80~1.40
A3

Mechanical properties of gradeA3

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
332(≥) 576(≥) 11 44 32 Solution and Aging,Annealing,Ausaging,Q+T,etc 144

Physical properties of grade A3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
196(≥) 396(≥) 11 34 13 Solution and Aging,Annealing,Ausaging,Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
388 617 342

A3 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Products

A3 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
A387 F5 & Grade 5 sheet Coil strip 0.5mmx200mmxC Coil or Strip Tons 3 Cold-Rolled+Annealed Enquiry
A387 F5 & Grade 5 Hot Coil stock Select Tons 3 Hot-Rolled+Annealed+black Enquiry