Steel, Bars and Forgings 2.0Cr - 10Ni - 14Co - 1.0Mo (0.15 - 0.19C) Vacuum Melted, Normalized and Overaged
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.13 | 0.17 | ||
Si | - | 0.10 | ||
Mn | - | 0.10 | ||
P | - | 0.008 | ||
S | - | 0.005 | ||
Ni | 9.50 | 10.50 | ||
Cr | 1.80 | 2.20 | ||
Al | - | 0.015 | ||
Cu | - | - | ||
Ti | - | 0.015 | ||
Fe | - | - | ||
N | - | 0.0015 | ||
Mo | 0.90 | 1.10 | ||
W | - | - | ||
O | - | 0.0015 | ||
Co | 13.50 | 14.50 |
Steel, Bars and Forgings 2.0Cr - 10Ni - 14Co - 1.0Mo (0.15 - 0.19C) Vacuum Melted, Normalized and Overaged
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
264 (≥) | 787 (≥) | 33 | 42 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
766 (≥) | 512 (≥) | 31 | 42 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
118 | 475 | 242 |
We can customize the production of AF 1410 grade, contact us for the best solution.