AMS 6481 Tool Die Steels

AMS 6481 - Specification & Application

Chemical composition(wt.%) of AMS 6481 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C(CarBon) - 0.35
Cr - 3.0
Mo - 1.0
V - 0.25

AMS 6481 - Detail

AMS 6481

Mechanical properties of grade AMS 6481

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
244 (≥) 922 (≥) 14 11 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade AMS 6481

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
129 (≥) 498 (≥) 41 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
952 991 527