CX-3 Special Alloy

Chemical composition%of the ladle analysis of gradeCX-3

C(%)W(%)Co(%)Ta(%)
5.1653.5116.025.33
CX-3
Density / (g/cm ^ 3) : 13.55 Hardness HRC: 85.0 σ bb/MPa: 1580 ~ 2280 Grain size/μ m: 4 ~ 5 Use for example: suitable for use in high temperature, such as used for hot pressing processing

Mechanical properties of gradeCX-3

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
242(≥) 472(≥) 11 43 43 Solution and Aging,Annealing,Ausaging,Q+T,etc 313

Physical properties of grade CX-3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
421(≥) 232(≥) 22 21 24 Solution and Aging,Annealing,Ausaging,Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
572 777 738

CX-3 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade