Standard Specification for Wrought Nitrogen Strengthened 22 Chromium - 13 Nickel - 5 Manganese - 2.5 Molybdenum Stainless Steel Alloy Bar and Wire for Surgical Implants (UNS S20910)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.06 | ||
Mn | 4.00 | 6.00 | ||
Si | - | 1.00 | ||
P | - | 0.04 | ||
S | - | 0.03 | ||
Cr | 20.50 | 23.50 | ||
Ni | 11.50 | 13.50 | ||
Mo | 1.50 | 3.00 | ||
N | 0.20 | 0.40 | ||
Nb | 0.10 | 0.30 | ||
V | 0.10 | 0.30 |
Standard Specification for Wrought Nitrogen Strengthened 22 Chromium - 13 Nickel - 5 Manganese - 2.5 Molybdenum Stainless Steel Alloy Bar and Wire for Surgical Implants (UNS S20910)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
595 (≥) | 316 (≥) | 21 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
424 (≥) | 927 (≥) | 11 | 34 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
271 | 538 | 861 |
We can customize the production of F 1314 S20910 grade, contact us for the best solution.