F 594 304L Stainless Steels to F 594 (2009)

F 594 304L - Specification & Application

  • F 594 (2009) - Standard Specification for Stainless Steel Nuts

Standard Specification for Stainless Steel Nuts

Chemical composition(wt.%) of F 594 304L grade: to F 594 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 8.00 12.0
N - 0.10

F 594 304L - Detail

Standard Specification for Stainless Steel Nuts

Mechanical properties of grade F 594 304L F 594 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
422 (≥) 684 (≥) 11 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade F 594 304L F 594 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
526 (≥) 125 (≥) 34 33 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
771 358 822
We can customize the production of F 594 304L grade, contact us for the best solution.
sales@specificsteel.com