GH2038 Stainless Steels to GB/T 14992 (2005)

GH2038 - Specification & Application

  • GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials

Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(wt.%) of GH2038 grade: to GB/T 14992 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Cr 10.0 12.5
Ni 18.0 21.0
Al - 0.50
Ti 2.30 2.80
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.020
B - 0.008

GH2038 - Detail

GH2038

Mechanical properties of grade GH2038 GB/T 14992 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
426 (≥) 394 (≥) 31 14 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade GH2038 GB/T 14992 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
234 (≥) 496 (≥) 12 13 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
537 628 116

Equivalent Grade

Equivalent Products

We can customize the production of GH2038 grade, contact us for the best solution.