C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | V(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
0.35~0.45 | 0.80~1.20 | 0.25~0.70 | ≤0.030 | ≤0.030 | 3.00~3.75 | ≤0.75 | 2.00~3.00 | 0.25~0.75 | ≤0.75 |
Proof strength Rp0.2(MPa) |
Tensile strength Rm(MPa) |
Impact energy KV(J) |
Elongation at fracture A(%) |
Reduction in cross section on fracture Z(%) |
As-Heat-Treated Condition | Brinell hardness(HBW) |
---|---|---|---|---|---|---|
582(≥) | 638(≥) | 23 | 12 | 12 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 122 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J/kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
479(≥) | 739(≥) | 31 | 42 | 13 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 211 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0)N/mm2 |
Creep rupture strength (10000h) (Rp1,0)N/mm2 |
|||||
783 | 513 | 846 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates/Sheets | Plates/Sheets | 0.08-200mm(T)*W*L | Forging,hot rolling and cold rolling | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Steel Bar | Round Bar,Flat Bar,Square Bar | Φ8-1200mm*L | Forging,hot rolling and cold rolling,Cast | Black,Rough Turning,Shot Blasting, |
Coil/Strip | Steel Coil/Steel Strip | 0.03-16.0x1200mm | Cold-Rolled&Hot-Rolled | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Pipes/Tubes | Seamless Pipes/Tubes,Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion,Cold Drawn,Welded | Annealed,Solution and Aging,Q+T,ACID-WASHED |