H12 Tool Die Steels

H12 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of H12 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.40
Si 0.80 1.20
Mn 0.20 0.40
Cr 4.75 5.50
Mo 1.25 1.75
V 0.10 0.50
W 1.00 1.70

H12 - Detail

Hot-Work Tool Steel

Mechanical properties of grade H12

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
852 (≥) 113 (≥) 21 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade H12

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
977 (≥) 589 (≥) 12 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
733 727 873

Equivalent Products

We can customize the production of H12 grade, contact us for the best solution.