H15410 Stainless Steels

H15410 - Specification & Application

Intake valve steel

Chemical composition(wt.%) of H15410 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.42 0.45
Si 0.15 0.30
Mn 1.25 1.75
P - 0.040
S - 0.05

H15410 - Detail

Intake valve steel

Mechanical properties of grade H15410

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
732 (≥) 476 (≥) 11 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade H15410

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
737 (≥) 967 (≥) 43 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
572 386 345