HFM 304S51 Stainless Steels to BS 3605-1

HFM 304S51 - Specification & Application

  • BS 3605-1 - Austenitic stainless steel pipes and tubes for pressure purposes. Specification for seamless tubes

Austenitic stainless steel pipes and tubes for pressure purposes. Specification for seamless tubes

Chemical composition(wt.%) of HFM 304S51 grade: to BS 3605-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 2.00
P - 0.04
S - 0.03
Cr 17.00 19.00
Mo - -
Ni 8.00 11.00

HFM 304S51 - Detail

Austenitic stainless steel pipes and tubes for pressure purposes. Specification for seamless tubes

Mechanical properties of grade HFM 304S51 BS 3605-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
469 (≥) 897 (≥) 22 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade HFM 304S51 BS 3605-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
424 (≥) 637 (≥) 22 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
858 198 212