HNV2 Stainless Steels

HNV2 - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of HNV2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40
Si 3.90
Mn 0.30
P
S
Cr 2.20

HNV2 - Detail

Steel for intake valves

Mechanical properties of grade HNV2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
782 (≥) 171 (≥) 32 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade HNV2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
132 (≥) 919 (≥) 24 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
273 481 941

Equivalent Products

We can customize the production of HNV2 grade, contact us for the best solution.