L5 Tool Die Steels

L5 - Specification & Application

Low Alloy Tool Steel

Chemical composition(wt.%) of L5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.90 1.10
Si 0.10 0.40
Mn 0.90 1.10
Cr 0.90 1.10
Mo 0.25 0.30
V - -
W - -

L5 - Detail

Low Alloy Tool Steel

Mechanical properties of grade L5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
831 (≥) 415 (≥) 44 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade L5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
283 (≥) 376 (≥) 22 44 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
998 127 957
We can customize the production of L5 grade, contact us for the best solution.