M41 Tool Die Steels

M41 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of M41 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.05 1.15
Si 0.15 0.50
Mn 0.20 0.60
P - 0.030
S - 0.030
Cr 3.75 4.50
Mo 3.25 4.25
V 1.75 2.25
W 6.25 7.00
Co 4.75 5.75

M41 - Detail

High-Speed Tool Steel

Mechanical properties of grade M41

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
294 (≥) 969 (≥) 34 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade M41

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
439 (≥) 267 (≥) 41 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
912 893 848