NA35 Stainless Steels to BS 2901-5

NA35 - Specification & Application

  • BS 2901-5 - Filler rods and wires for gas-shielded arc weldingSpecification for nickel and nickel alloys

Filler rods and wires for gas-shielded arc weldingSpecification for nickel and nickel alloys

Chemical composition(wt.%) of NA35 grade: to BS 2901-5

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 3.50 4.50
Mn - 1.50
P - 0.030
S - 0.030
Cr - -
Mo - -
Ni - remaining
Cu 28.00 34.00

NA35 - Detail

Filler rods and wires for gas-shielded arc weldingSpecification for nickel and nickel alloys

Mechanical properties of grade NA35 BS 2901-5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
721 (≥) 358 (≥) 41 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade NA35 BS 2901-5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
189 (≥) 876 (≥) 42 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
152 276 487

Equivalent Products

We can customize the production of NA35 grade, contact us for the best solution.
sales@specificsteel.com