NCF601 Stainless Steels to D 3531 (2007)

NCF601 - Specification & Application

  • D 3531 (2007) - Corrosion - resisting and heat - resisting superalloy bars
  • D 3532 (2002) - Corrosion - resisting and heat - resisting superalloy plates and sheets

Corrosion - resisting and heat - resisting superalloy plates and sheets

Chemical composition(wt.%) of NCF601 grade: to D 3531 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.50
Mn - 1.00
P - 0.030
S - 0.015
Cr 21.00 25.00
Ni 58.00 63.00
Cu - 1.00
Al 1.00 1.70
Ti - -
Fe - remaining

NCF601 - Detail

Corrosion - resisting and heat - resisting superalloy plates and sheets

Mechanical properties of grade NCF601 D 3531 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
344 (≥) 567 (≥) 34 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade NCF601 D 3531 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
925 (≥) 612 (≥) 32 44 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
593 132 798

Equivalent Products