C(%) | Si(%) | Mn(%) | P(%) | S(%) |
---|---|---|---|---|
≤0.20 | ≤0.30 | 0.40~0.70 | ≤0.035 | ≤0.035 |
Steel thickness/mm: more than 16
The yield point | σ s frequency/MPa: 235
Tensile depth | σ b frequency/MPa: 390
Elongation | δ frequency / (%) 5:26
Impact absorption power AKV/J | testing temperature / ℃ : 0
Impact absorption power AKV/J | longitudinal frequency/J | : 27
Impact absorption power AKV/J | time frequency/J | : 27
180 ° of cold bending test | d-apex diameter, a-the following steel thickness thickness when/mm | than 16: d = 1.5 a
180 ° of cold bending test | d-apex diameter, a-the following steel thickness thickness when/mm | > 16: d = 2.5 a
Proof strength Rp0.2(MPa) |
Tensile strength Rm(MPa) |
Impact energy KV(J) |
Elongation at fracture A(%) |
Reduction in cross section on fracture Z(%) |
As-Heat-Treated Condition | Brinell hardness(HBW) |
---|---|---|---|---|---|---|
439(≥) | 447(≥) | 12 | 43 | 43 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 111 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J/kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
731(≥) | 172(≥) | 41 | 23 | 22 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 434 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0)N/mm2 |
Creep rupture strength (10000h) (Rp1,0)N/mm2 |
|||||
285 | 586 | 265 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates/Sheets | Plates/Sheets | 0.08-200mm(T)*W*L | Forging,hot rolling and cold rolling | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Steel Bar | Round Bar,Flat Bar,Square Bar | Φ8-1200mm*L | Forging,hot rolling and cold rolling,Cast | Black,Rough Turning,Shot Blasting, |
Coil/Strip | Steel Coil/Steel Strip | 0.03-16.0x1200mm | Cold-Rolled&Hot-Rolled | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Pipes/Tubes | Seamless Pipes/Tubes,Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion,Cold Drawn,Welded | Annealed,Solution and Aging,Q+T,ACID-WASHED |
Steel grade | Dimension | Shape | Unit | Quantity | Delivery state | Query |
---|---|---|---|---|---|---|
SkD-11 Round Bar Stock | Φ30-Φ350 | Round Bar | Kgs | 3102 | Hot-Rolled+Annealed+black | Enquiry |
17-4PH Coil Stock | 0.08*200mm | Coil or Strip | Kgs | 1623 | Cold-Rolled+Annealed | Enquiry |
D2 Round bar | Φ25-Φ380mm | Round Bar | Kgs | 45325 | Hot-Rolled+Annealed+black | Enquiry |
Cr8 flat bar | 12*355*L | Flat or Square bar | Kgs | 3965 | Forged+Annealed+black | Enquiry |
17-4PH Round Bar | Φ5-300mm*L | Round Bar | Kgs | 46958 | Hot-Rolled+Annealed+black | Enquiry |
17-4PH plate | 8-45*1200*3000mm | Plate or Sheet | Tons | 4.9 | Hot-Rolled+Annealed+black | Enquiry |
Cr12MoV | 12-160(T)*310-610(W)*L | Plate or Sheet | Tons | 12.38 | Hot-Rolled+Annealed+black | Enquiry |
1.2601 | 12-160(T)*310-610(W)*L | Plate or Sheet | Tons | 11.22 | Hot-Rolled+Annealed+black | Enquiry |
IncoloyA-286 / GH 2132 Stock | Φ8-65mm*L | Round Bar | Kgs | 489 | Hot-Rolled+Annealed+black | Enquiry |
Incoloy800 round bar | Φ115*1400 | Round Bar | Kgs | 169 | Hot-Rolled+Annealed+black | Enquiry |
17-7PH / 631 Coil & Strip, Sheet Stock | 0.3-3.0*10-180mm | Coil or Strip | Kgs | 1236.22 | Cold-Rolled+Annealed | Enquiry |
X22CrMoV12-1 / 1.4923 | Φ17mm | Round Bar | Kgs | 300 | Hot-Rolled+Annealed+black | Enquiry |
1.2083 Forged Plate | T:105-185mm*W:510*L | Plate or Sheet | Tons | 26 | Forged+QT | Enquiry |
X22CrMoV12-1 / 1.4923 | Φ30mm | Round Bar | Kgs | 300 | Hot-Rolled+Annealed+black | Enquiry |
1.4882 strip/sheet/plate stock | 3.5x200x1000-2000mm | Coil or Strip | Kgs | 200 | Cold-Rolled+Annealed | Enquiry |
A387 F5 & Grade 5 sheet Coil strip | 0.5mmx200mmxC | Coil or Strip | Tons | 3 | Cold-Rolled+Annealed | Enquiry |
A387 F5 & Grade 5 Hot Coil stock | Select | Tons | 3 | Hot-Rolled+Annealed+black | Enquiry | |
T45Cr5Si3 Round Bar | Dia.40mm | Round Bar | Kgs | 500 | Hot-Rolled+Annealed+black | Enquiry |
UNS K30960(VIM+ESR) Bright Round Bar | Dia.22mm | Round Bar | Kgs | 50 | Hot-Rolled+Annealed+black | Enquiry |
SA-437 Grade B4B/SUS 616 /422 Forged Bar | Dia.160xL | Round Bar | Kgs | 2120 | Forged+QT | Enquiry |