  • SAE AMS 5399D (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution Heat Treated

Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution Heat Treated

Chemical composition(wt.%) of Rene 41 grade: to SAE AMS 5399D (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 0.25
Mn - 0.25
Cr - 19.00
Ni - remaining
Mo - 10.00
Co - 11.00
W - -
Al - 1.50
Cu - -
Ti - 3.10
Fe - 1.80
B - 0.005

Rene 41 - Detail

Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution Heat Treated

Mechanical properties of grade Rene 41 SAE AMS 5399D (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
393 (≥) 726 (≥) 43 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade Rene 41 SAE AMS 5399D (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
247 (≥) 863 (≥) 21 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
144 297 769