S21400 Stainless Steels

S21400 - Specification & Application

Chemical compositions of SAE wrought stainless steels

Chemical composition(wt.%) of S21400 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si 0.30 1.00
Mn 14.5 16.0
P - 0.045
S - 0.03
Cr 17.0 18.5
Ni - 1.00
N - 0.35

S21400 - Detail

S21400

Mechanical properties of grade S21400

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
722 (≥) 739 (≥) 31 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade S21400

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
919 (≥) 143 (≥) 33 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
342 348 239