S21800 Stainless Steels

S21800 - Specification & Application

Austenitic Chromium Nickel Manganese Stainless Steel

Chemical composition(wt.%) of S21800 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si 3.50 4.50
Mn 7.00 9.00
P - 0.04
S - 0.03
Cr 16.0 18.0
Ni 8.00 9.00
N 0.08 0.18

S21800 - Detail

S21800

Mechanical properties of grade S21800

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
944 (≥) 526 (≥) 33 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade S21800

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
848 (≥) 482 (≥) 11 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
913 158 352

Equivalent Products

We can customize the production of S21800 grade, contact us for the best solution.