S30200 Stainless Steels

S30200 - Specification & Application

Austenitic Chromium Nickel Stainless Steel

Chemical composition(wt.%) of S30200 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 6.00 8.00

S30200 - Detail

S30200

Mechanical properties of grade S30200

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
452 (≥) 719 (≥) 13 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade S30200

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
125 (≥) 145 (≥) 11 34 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
386 423 329
We can customize the production of S30200 grade, contact us for the best solution.