S44003 Stainless Steels

S44003 - Specification & Application

S44003

Chemical composition(wt.%) of S44003 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.75 0.95
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.0 18.0
Mo - 0.75

S44003 - Detail

S44003

Mechanical properties of grade S44003

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
819 (≥) 552 (≥) 44 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade S44003

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
891 (≥) 533 (≥) 11 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
713 313 959

Equivalent Products

We can customize the production of S44003 grade, contact us for the best solution.