S63014 Stainless Steels

S63014 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of S63014 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.45
Si 2.75 3.25
Mn 0.80 1.30
P - 0.040
S - 0.030
Cr 18.0 20.0
Ni 7.50 8.50

S63014 - Detail

Steel for exhaust valves

Mechanical properties of grade S63014

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
425 (≥) 996 (≥) 21 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade S63014

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
878 (≥) 857 (≥) 31 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
421 839 789