SA-666 S30451 Stainless Steels to SA-666

SA-666 S30451 - Specification & Application

  • SA-666 - Specification for Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar

Specification for Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar

Chemical composition(wt.%) of SA-666 S30451 grade: to SA-666

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 10.5
N 0.10 0.16

SA-666 S30451 - Detail

Specification for Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar

Mechanical properties of grade SA-666 S30451 SA-666

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
246 (≥) 471 (≥) 24 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade SA-666 S30451 SA-666

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
445 (≥) 745 (≥) 44 34 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
335 869 275