SA-688 S30451 Stainless Steels to SA-688/SA-688M

SA-688 S30451 - Specification & Application

  • SA-688/SA-688M - Specification for Welded Austenitic Stainless Steel Feedwater Heater Tubes

Specification for Welded Austenitic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of SA-688 S30451 grade: to SA-688/SA-688M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 10.5
N 0.10 0.16

SA-688 S30451 - Detail

Specification for Welded Austenitic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade SA-688 S30451 SA-688/SA-688M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
369 (≥) 392 (≥) 31 44 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade SA-688 S30451 SA-688/SA-688M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
244 (≥) 347 (≥) 43 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
558 373 277